Size | Dia. : 3 mm - 600 mm |
Material | GR1 GR2 GR3 GR4 GR5 GR7 GR9 GR23, etc. |
Standard | ASTM B348, ASTM F67, AMS 4928, ASTM F136,etc. |
Surface | Black, Pickling, Sand-blasting, Polished |
Shape | Square Bar, Round Bar, Hexagonal Bar, etc. |
Condition | Cold rolled(Y), Hot rolled(R), Annealed (M), Quenching (C) |
TNTI stocks a wide range of titanium rod, including a complete line of commercially pure and medical titanium rod. Titanium connecting rod, titanium rod in femur, titanium welding rod, titanium filler rod, titanium threaded rod, Nitinol rod etc, can all be met. It can be supplied in random lengths or cut into fixed lengths, according to your precise dimensions.
Titanium is highly resistant to chloride-containing media, practically all salt solutions, seawater, a range of acids, organic and inorganic chemicals and gases. The high environmental resistance is primarily based on a very thin, tenacious and highly protective surface oxide film. The oxide film provides high resistance to erosion in high velocity process streams. It is non-magnetic and characterized by a high melting point, high strength-to-weight ratio and a low modulus of elasticity.Chemical processing, Medical instruments, Aerospace, Industry, Navigation, Smelting, Chemical plants, Machinery and equipment, Electroplating equipment, Precision instruments standard parts, Titanium wind leaf in power used, etc.
Chemical requirements (Nominal %)
|
N |
C |
H |
Fe |
O |
Al |
V |
Pa |
Mo |
Ni |
Ti |
Gr 1 |
0.03 |
0.08 |
0.015 |
0.20 |
0.18 |
/ |
/ |
/ |
/ |
/ |
Remaining |
Gr 2 |
0.03 |
0.08 |
0.015 |
0.30 |
0.25 |
/ |
/ |
/ |
/ |
/ |
Remaining |
Gr 3 |
0.05 |
0.08 |
0.015 |
0.30 |
0.35 |
/ |
/ |
/ |
/ |
/ |
Remaining |
Gr 4 |
0.05 |
0.08 |
0.015 |
0.50 |
0.40 |
/ |
/ |
/ |
/ |
/ |
Remaining |
Gr 5 |
0.05 |
0.08 |
0.015 |
0.40 |
0.20 |
5.5~6.75 |
3.5~4.5 |
/ |
/ |
/ |
Remaining |
Gr 7 |
0.03 |
0.08 |
0.015 |
0.30 |
0.25 |
/ |
/ |
0.12~0.25 |
/ |
/ |
Remaining |
Gr 9 |
0.03 |
0.08 |
0.015 |
0.25 |
0.15 |
2.5~3.5 |
2.0~3.0 |
/ |
/ |
/ |
Remaining |
Gr12 |
0.03 |
0.08 |
0.015 |
0.30 |
0.25 |
/ |
/ |
/ |
0.2~0.4 |
0.6~0.9 |
Remaining |
Mechanical requirements
Grade |
Tensil strength (min) |
Yeild strength (min) |
Elongation(%) |
||
ksi |
MPa |
ksi |
MPa |
||
1 |
35 |
240 |
20 |
138 |
24 |
2 |
50 |
345 |
40 |
275 |
20 |
3 |
65 |
450 |
55 |
380 |
18 |
4 |
80 |
550 |
70 |
483 |
15 |
5 |
130 |
895 |
120 |
828 |
10 |
7 |
50 |
345 |
40 |
275 |
20 |
9 |
90 |
620 |
70 |
438 |
15 |
12 |
70 |
438 |
50 |
345 |
18 |
Features :